Polymer Property : Volume Resistivity = 3.20e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.20e+11 ohm-cm

@Temperature 350 °C
3.20e+11 ohm-cm

@Temperature 662 °F
Schott AF 45 Thin Borosilicate Glass
AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc..