Electrical Properties Metric English Comments
Volume Resistivity 3.10e+6 ohm-cm

@Temperature 350 °C
3.10e+6 ohm-cm

@Temperature 662 °F
Schott BOROFLOAT® Borosilicate Float Glass
This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting fro..