Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 250000 ohm-cm @Temperature 350 °C |
>= 250000 ohm-cm @Temperature 662 °F |
|
Schott ROBAX® Glass Ceramic ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s.. |