Electrical Properties Metric English Comments
Volume Resistivity >= 200000 ohm-cm

@Temperature 350 °C
>= 200000 ohm-cm

@Temperature 662 °F
Schott Dark ROBAX® Glass Ceramic
Dark ROBAX® is an infra-red transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in rolle..
Volume Resistivity 200000 ohm-cm

@Temperature 350 °C
200000 ohm-cm

@Temperature 662 °F
DIN 52326
Schott Nextrema® 724-3 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..