Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.50e+8 ohm-cm @Temperature 350 °C |
2.50e+8 ohm-cm @Temperature 662 °F |
|
Schott Glass 8270 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elem.. |
|||
Volume Resistivity | 2.50e+8 ohm-cm @Temperature 350 °C |
2.50e+8 ohm-cm @Temperature 662 °F |
|
Corning 7056 Alkali Borosilicate Crushed/Powdered Glass Crushed/Powdered glass available in mesh sizes 4 through 325 and can be customized. Used primarily as a Kovar Sealing Glass. This product is used in MOEMS applications. Information provided by Corn.. |
|||
Volume Resistivity | 2.50e+8 ohm-cm @Temperature 112 °C |
2.50e+8 ohm-cm @Temperature 234 °F |
cured 2 hours @ 93°C |
Abatron AboCast 8110-7/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |