Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.50e+7 ohm-cm @Temperature 250 °C |
2.50e+7 ohm-cm @Temperature 482 °F |
|
Schott Glass 8245 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, minimum X-ray absorption, low self radiation, good insulator X-ray tubes, video-frequency tubes, photomultiplier tubes The heavy metal.. |
|||
Volume Resistivity | 2.50e+7 ohm-cm @Temperature 350 °C |
2.50e+7 ohm-cm @Temperature 662 °F |
|
Schott Glass 8688 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
Volume Resistivity | 2.50e+7 ohm-cm @Temperature 250 °C |
2.50e+7 ohm-cm @Temperature 482 °F |
|
Schott DUROBAX® clear Neutral Glass Tubing Neutral glass tubing, chemically highly resistant Syringes, cartridges, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is.. |