Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.40e+15 ohm-cm @Temperature 100 °C |
2.40e+15 ohm-cm @Temperature 212 °F |
|
Advanced Ceramics ACL 2087 Lithium Alumino-Silicate A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL) |