Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.60e+9 ohm-cm @Temperature 500 °C |
1.60e+9 ohm-cm @Temperature 932 °F |
|
Schott AF 45 Thin Borosilicate Glass AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc.. |
|||
Volume Resistivity | 1.60e+9 ohm-cm @Temperature 250 °C |
1.60e+9 ohm-cm @Temperature 482 °F |
|
Schott Glass 8337B Borosilicate Glass Borosilicate glass for sealing to Kovar metal and tungsten, highly UV-transmitting photomultiplier and UV detectors The heavy metal content for the elements lead, cadmium, mercury, and hexavalent .. |