Polymer Property : Volume Resistivity = 1.60e+7 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+7 ohm-cm

@Temperature 250 °C
1.60e+7 ohm-cm

@Temperature 482 °F
Schott Glass 8625 Biocompatible Glass
Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S..
Volume Resistivity 1.60e+7 ohm-cm

@Temperature 250 °C
1.60e+7 ohm-cm

@Temperature 482 °F
DIN 52326
Schott Nextrema® 712-6 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..