Polymer Property : Volume Resistivity = 1.60e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+11 ohm-cm

@Temperature 250 °C
1.60e+11 ohm-cm

@Temperature 482 °F
Schott Glass 8651 Sealing Glass
Tungsten sealing glass Power diodesInformation provided by SCHOTT AG.
Volume Resistivity 1.60e+11 ohm-cm

@Temperature 250 °C
1.60e+11 ohm-cm

@Temperature 482 °F
Corning Pyrex® 7740 Borosilicate Glass
Pyrex® sheet provides unique chemical, thermal, mechanical, and optical properties. Available in thicknesses from 3/32 inches to 2.25 inches. Tempering increases temperature and pressure capabili..