Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.50e+15 ohm-cm @Temperature 300 °C |
>= 1.50e+15 ohm-cm @Temperature 572 °F |
|
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor .. |