Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.30e+6 ohm-cm @Temperature 250 °C |
1.30e+6 ohm-cm @Temperature 482 °F |
|
Corning 7070 Lithia Potash Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Devitrifies before reaching a softening point. Used for sealing and other applications.Information provided by Corning Incorporated. |