Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+18 ohm-cm @Temperature 23.0 °C |
1.00e+18 ohm-cm @Temperature 73.4 °F |
DC; DIN 40634 or VDE 0345 in air or ASTM D257 |
Mitsubishi Hostaphan® WN, 190 micron Nominal Thickness Translucent White Polyethylene Terephthalate Film Hostaphan® WN is a white film made of polyethylene terephthalate (PET) and is well suited for electrical insulating of machines and appliances. The high dielectric strength and large volume resis.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm @Temperature 50.0 °C |
1.00e+18 ohm-cm @Temperature 122 °F |
ASTM D257 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm @Temperature 100 °C |
1.00e+18 ohm-cm @Temperature 212 °F |
ASTM D257 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm @Temperature 90.0 °C |
1.00e+18 ohm-cm @Temperature 194 °F |
in oil; ASTM D257 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm @Temperature 90.0 °C |
1.00e+18 ohm-cm @Temperature 194 °F |
in oil; ASTM D257 |
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm @Temperature 90.0 °C |
1.00e+18 ohm-cm @Temperature 194 °F |
in oil; ASTM D257 |
DuPont™ Nomex® Type 993, 60 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |