Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 1.0 ohm-cm @Temperature 20.0 °C |
<= 1.0 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Volume Resistivity | <= 1.0 ohm-cm @Temperature 20.0 °C |
<= 1.0 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |