Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 0.0090 ohm-cm @Treatment Temp. 65.0 °C, Time 7200 sec |
<= 0.0090 ohm-cm @Treatment Temp. 149 °F, Time 2.00 hour |
|
Parker Chomerics CHO-BOND 584-29 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Volume Resistivity | <= 0.0090 ohm-cm @Temperature 23.0 °C, Time 259000 sec |
<= 0.0090 ohm-cm @Temperature 73.4 °F, Time 72.0 hour |
|
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |
|||
Volume Resistivity | <= 0.0090 ohm-cm @Temperature 23.0 °C, Time 259000 sec |
<= 0.0090 ohm-cm @Temperature 73.4 °F, Time 72.0 hour |
|
Epoxy Technology EPO-TEK® EJ2189-LV Electrically Conductive Epoxy Low Viscosity, two component room temp curing conductive epoxyInformation Provided by Epoxy Technology |