Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 0.00050 ohm-cm @Temperature 150 °C, Time 3600 sec |
<= 0.00050 ohm-cm @Temperature 302 °F, Time 1.00 hour |
|
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |
|||
Volume Resistivity | <= 0.00050 ohm-cm @Temperature 150 °C, Time 3600 sec |
<= 0.00050 ohm-cm @Temperature 302 °F, Time 1.00 hour |
|
Epoxy Technology EPO-TEK® EJ2189-LV Electrically Conductive Epoxy Low Viscosity, two component room temp curing conductive epoxyInformation Provided by Epoxy Technology |