Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Saturation Flux Density, Bmax | 8800 Gauss | 8800 Gauss | |
Goodfellow Iron 40/Nickel 38/Boron 18 Alloy Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow. |