Magnetic Saturation Flux Density, Bmax 17000 Gauss
17000 Gauss
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar
Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope..