Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Saturation Flux Density, Bmax | 16350 Gauss | 16350 Gauss | Saturate Magnetism |
International Mold Steel NAK55 Precipitation Hardened Mold Steel Description: NAK55 is a precipitation, or age-hardened mold steel with a through hardness of approximately 40 HRc. NAK55 is ideal for use in plastic and rubber molds and other applications where imp.. |