Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Saturation Flux Density, Bmax | 15100 Gauss | 15100 Gauss | Magnetizing field of 25 Oe. |
FloMet Fe-3% Si Soft Magnetic Alloy FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |