Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Saturation Flux Density, Bmax | 13000 Gauss | 13000 Gauss | Magnetic Induction |
Pacific Sintered Materials F-241-T Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE V, CLASS AAll information provided by Pac.. |
|||
Magnetic Saturation Flux Density, Bmax | 13000 Gauss | 13000 Gauss | Magnetic Induction |
Pacific Sintered Materials FS-1601 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |
|||
Magnetic Saturation Flux Density, Bmax | 13000 Gauss | 13000 Gauss | Magnetic Induction |
Pacific Sintered Materials FS-1602 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |