Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.90e+12 ohm-cm | 9.90e+12 ohm-cm | ASTM D257 |
Teknor Apex APEX® 80328-YFR Polyvinyl Chloride, Flexible Notes: 75°C Insulation; RoHS Compliant Features: Flame Retardant; Good UV Resistance Uses: Cable Jacketing; InsulationAgency Ratings: UL QMTT2 .E73402 Forms: Pellets Wire Types: TWInformation Pro.. |