Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.80e+11 ohm-cm | 9.80e+11 ohm-cm | ASTM D247 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |