Electrical Properties Metric English Comments
Volume Resistivity 9.50e+15 ohm-cm
9.50e+15 ohm-cm
IEC 93
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..