Polymer Property : Volume Resistivity = 8.80e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 8.80e+15 ohm-cm
8.80e+15 ohm-cm
Cured property; ASTM D257
Aptek 2100-A/B Urethane Encapsulant and/or Potting Compound
General purpose encapsulant and potting compound. Outstanding hydrolytic stability. Excellent adhesion to components/circuit boards. Low modulus, low stress. Field proven for military and space appl..