Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.80e+13 ohm-cm | 8.80e+13 ohm-cm | ASTM D257 |
Teknor Apex APEX® 80853-B Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; Oil Resistant Uses: Insulation; Wire and Cable Applications Agency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire T.. |