Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.40e+14 ohm-cm | 8.40e+14 ohm-cm | ASTM D257 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |