Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.20e+20 ohm-cm | 8.20e+20 ohm-cm | ASTM D257 |
Manifattura Cattaneo RULON® J Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |