Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.20e+13 ohm-cm | 8.20e+13 ohm-cm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |