Polymer Property : Volume Resistivity = 8.00e+18 ohm-cm
Polymer Property :
Volume Resistivity =
8.00e+18 ohm-cm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Volume Resistivity
8.00e+18
ohm-cm
8.00e+18
ohm-cm
ASTM D257
Adamas Adalon® 403 PTFE, 15% Polyimide
Information provided by Adamas, HPM