Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.50e+11 ohm-cm | 7.50e+11 ohm-cm | ASTM D247 |
Plenco 4300 Phenolic, Granular, Injection Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |