Polymer Property : Volume Resistivity = 7.40e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 7.40e+15 ohm-cm
7.40e+15 ohm-cm
70°C for 1,000 hrs; JIS-K-6249
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b..
Volume Resistivity 7.40e+15 ohm-cm
7.40e+15 ohm-cm
IEC 93
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET
PBT + PET, injection-molding grade containing 30% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin..