Polymer Property : Volume Resistivity = 7.20e+10 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 7.20e+10 ohm-cm
7.20e+10 ohm-cm
Industrial Laminates/Norplex MC320LE Cotton Fabric
Description: Grade MC320LE is a fine weave bleached cotton phenolic composite that has excellent machining characteristics and low moisture absorption. Applications include marine applications, term..
Volume Resistivity 7.20e+10 ohm-cm
7.20e+10 ohm-cm
Tra-Con Tra-Bond 927-1 Polysulfide Adhesive
TRA-BOND 927-1 thermally conductive polysulfide adhesive is designed for heat sink bonding applications. Information provided by Tra-Con Inc.