Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.00e+10 ohm-cm | 7.00e+10 ohm-cm | |
Pyrotek TS-83 Thermoset Electrical Insulation Product (Nema Grade: LE) Linen reinforcement, Phenolic resin, Tan / Black color. Good electrical and high mechanical strength. Moisture resistant.Information provided by Pyrotek. |
|||
Volume Resistivity | 7.00e+10 ohm-cm | 7.00e+10 ohm-cm | |
LE Phenolic Laminate Linen based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many st.. |