Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.0 - 7.0 ohm-cm | 3.0 - 7.0 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX WX94736 PBT LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel. |