Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.90e+16 ohm-cm | 6.90e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 745 PBT 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
Volume Resistivity | 6.90e+16 ohm-cm | 6.90e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific) 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
Volume Resistivity | 6.90e+16 ohm-cm | 6.90e+16 ohm-cm | ASTM D 257 |
Zylog Neoplast® 243 HOFR Thermoplastic Vulcanizate Neoplast 243 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize.. |