Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.90e+14 ohm-cm | 6.90e+14 ohm-cm | ASTM D257 |
PolyOne Geon™ Vinyl Wire & Cable E1330I Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Volume Resistivity | 6.90e+14 ohm-cm | 6.90e+14 ohm-cm | |
Pyrotek ISOMAG® 175 Structural Insulation Board Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr.. |
|||
Volume Resistivity | 6.90e+14 ohm-cm | 6.90e+14 ohm-cm | IEC 60167 |
Lucobit Lucofin® 7440 HFFR EBA MDH Cable Sheathing Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and.. |