Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 58000 ohm-cm | 58000 ohm-cm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |