Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.90e+12 ohm-cm | 5.90e+12 ohm-cm | ISO.93 DIN.53482 |
Omnia Plastica PEI Polyetherimide This high performance engineering plastic is a non-reinforced self-extinguishing amorphous polymer with high thermal, electrical and mechanical properties which are typical of a crystalline polymer... |
|||
Volume Resistivity | 5.90e+12 ohm-cm | 5.90e+12 ohm-cm | ASTM D247 |
Plenco 2369 Phenolic, Granular, Transfer Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |