Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.60e+14 ohm-cm | 5.60e+14 ohm-cm | |
Momentive Performance Materials RTV577 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Volume Resistivity | 5.60e+14 ohm-cm | 5.60e+14 ohm-cm | ASTM D247 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |