Polymer Property : Volume Resistivity = 5.50e+12 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 5.50e+12 ohm-cm
5.50e+12 ohm-cm
ASTM D257
PolyOne Geon™ Vinyl Flexible R7426A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne