Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 450 ohm-cm | 450 ohm-cm | |
LATI Latilub 87/28-17ST K/15 PC, 15% Carbon Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polycarbonate (PC). Silicone / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Volume Resistivity | 450 ohm-cm | 450 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing |