Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4100 ohm-cm | 4100 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow. |