Volume Resistivity 410 ohm-cm
410 ohm-cm
EVA/NBR Strippable Compounds
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..