Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.50e+15 ohm-cm | 4.50e+15 ohm-cm | ASTM D257 |
PolyOne Geon™ Vinyl Flexible R3792C Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Volume Resistivity | 4.50e+15 ohm-cm | 4.50e+15 ohm-cm | |
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released.. |