Volume Resistivity 4.40e+14 ohm-cm
4.40e+14 ohm-cm
Momentive Performance Materials RTV8262 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr..
Volume Resistivity 4.40e+14 ohm-cm
4.40e+14 ohm-cm
Momentive Performance Materials RTV60 Silicone Rubber Compound for High Temperature, Red
RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa..
Volume Resistivity 4.40e+14 ohm-cm
4.40e+14 ohm-cm
ASTM D247
Plenco 1500 Polyester, Granular, Compression Molded