Volume Resistivity 4.10e+6 ohm-cm
4.10e+6 ohm-cm
CTM E043
Nanocyl PLASTICYL™ PP2001 Polypropylene with 2 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..