Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.10e+10 ohm-cm | 4.10e+10 ohm-cm | ISO.93 DIN.53482 |
Omnia Plastica PEEK Polyetheretherketone Semicrystalline polymer. Material with high mechanical and thermal properties, up to 240°C. It resists to creep under load and to wear, its friction coefficient is low. The temperature resistance w.. |