Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.80e+16 ohm-cm | 3.80e+16 ohm-cm | |
Tra-Con Tra-Bond 2126 Black Opaque Epoxy Adhesive TRA-BOND 2126 is recommended for those modern photographic, industrial, and laboratory bonding and laminating applications where an easy-to-use, black (opaque) epoxy adhesive system with high perfor.. |