Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.70e+14 ohm-cm | 3.70e+14 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 85T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |